Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 143 MPa | 20700 psi | ASTM D695 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |