Polymer Property : Compressive Strength = 142.2 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.9807 MPa
142.2 psi
to 25% compression
Pyrotek LUMIFELT AL20 High Temperature Kevlar® Felt
Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and..
Compressive Strength 0.9807 MPa
142.2 psi
to 4% compression
Pyrotek LUMIFELT AL20L High Temperature Kevlar® Felt
Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and..