Compressive Strength 9.10 MPa
1320 psi
ASTM D1621
Dow BETAFOAM™ 87100/87124
BETAFOAM™ 87100/87124 is a high-density, all-water blown rigid polyurethane foam. These components were engineered to produce a foam for increasing stiffness of body structure cavities. Foam is p..