Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 12.4 MPa | 1800 psi | ASTM D695 |
ScanTube THV Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 12.4 MPa @Temperature 815 °C |
1800 psi @Temperature 1500 °F |
Cold Crush Strength |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |