Polymer Property : Compressive Strength = 116.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 116.6 MPa
16910 psi
Henkel Hysol EA 956 Paste Adhesive System
Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up