Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 79.01 MPa | 11460 psi | 2% Def.; ISO 604 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |