Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 10900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 75.2 MPa
10900 psi
2% Def.; ISO 604
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet)
KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. ..
Compressive Strength 75.0 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
ASTM D695
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Compressive Strength 75.0 MPa
10900 psi
Cold Crushing Strength
Gouda Vuurvast AK 70 KP Dense Refractory Brick
Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average ..
Compressive Strength 75.0 MPa
10900 psi
Cold Crushing Strength
Gouda Vuurvast AK 99 Dense Refractory Brick
Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T..
Compressive Strength 75.0 MPa
10900 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Compressive Strength 75.0 MPa

@Time 36.0 sec
10900 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Compressive Strength 75.0 MPa

@Time 36.0 sec
10900 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
Compressive Strength 75.2 MPa
10900 psi
ASTM D-695
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures
RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling a..
Compressive Strength >= 75.0 MPa
>= 10900 psi
Ambient
China-Yixing Longly Refractories Seggar Semi-Corundum-Mullite
Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine..
Compressive Strength 75.2 MPa
10900 psi
Abatron AboCast 8103-14 One-Component Epoxy
AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting..