Mechanical Properties Metric English Comments
Compressive Strength >= 0.750 MPa
>= 109 psi
perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..