Polymer Property : Compressive Strength = 105 MPa
Polymer Property :
Compressive Strength =
105 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
90.0
-
105
MPa
13100
-
15200
psi
GB/T 1040
Beijing Evergrow Resources MoS2 Filled Nylon