Polymer Property : Compressive Strength = 1.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.40 MPa
203 psi
EN 1094-5: 1995
Skamol Group Moler HIPOR Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Compressive Strength 1.40 MPa
203 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Compressive Strength 1.40 MPa
203 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..
Compressive Strength 1.40 MPa
203 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..