Mechanical Properties Metric English Comments
Compressive Strength 0.700 - 1.30 MPa
102 - 189 psi
Cold Crushing Strength
Gouda Vuurvast GI 23 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.