Polymer Property : Compressive Strength = 1.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.30 MPa
189 psi
90 g/l
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..
Compressive Strength >= 1.30 MPa
>= 189 psi
@ 20 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Compressive Strength >= 1.30 MPa
>= 189 psi
@ 20 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Compressive Strength 1.30 MPa
189 psi
EN 1094-5: 1995
Skamol Group V-1100 375 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Compressive Strength 1.30 MPa
189 psi
EN 1094-5: 1995
Skamol Group V-LITE 375 Vermiculite Insulating Brick
V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica..
Compressive Strength 1.30 MPa

@Temperature 700 °C
189 psi

@Temperature 1290 °F
Unifrax Excelfrax® 1900 Panel Microporous Insulation
Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo..
Compressive Strength 1.30 MPa
189 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZ-23HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 1.30 MPa
189 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZP-23L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength >= 1.30 MPa
>= 189 psi
perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Compressive Strength >= 1.30 MPa
>= 189 psi
perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..