Polymer Property : Compressive Strength = 0.560 MPa
Polymer Property :
Compressive Strength =
0.560 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
0.560
MPa
81.2
psi
12 g/l
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding
High quality processingHigh strengthLow wasteFast moulding cycles