Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.421 MPa | 61.0 psi | 10% Deformation; Green |
Unifrax Fiberfrax® Duraboard® RG Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |