Mechanical Properties Metric English Comments
Compressive Strength 0.290 MPa
42.0 psi
5% Deformation; Green
Unifrax Fiberfrax® Duraboard® 3000 Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.290 MPa
42.0 psi
5% Deformation; Green
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Compressive Strength 0.290 MPa
42.0 psi
at 25%, Horizontal; ASTM D3575, Suffix D
Dow STRANDFOAM™ EA 1600 Polypropylene Foam
STRANDFOAM™ EA 1600 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra..