Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 0.0552 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12050 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12054 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12056 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12062 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
10% Compression, Deflection
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.0552 MPa
8.00 psi
10% Compression, Deflection
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 - 0.0827 MPa
8.00 - 12.0 psi
Deflection
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12046 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12048 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Compressive Strength 0.0552 MPa
8.00 psi
Force Deflection; ASTMD3574-D
3M 6035PC 12049 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series)
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and..
Copyright © lookpolymers.com All Rights Reserved