Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Compressive Strength | 0.0241 - 0.0448 MPa | 3.50 - 6.50 psi | Deflection |
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |