Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 66.7 MPa | 9670 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BTE30-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 66.7 MPa | 9670 psi | ASTM D638 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Tensile Strength | 66.7 MPa | 9670 psi | ASTM D638 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |