Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.58 MPa | 955 psi | Silicone Property; ASTM D412 |
Arlon LW202R##-P0 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 2 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |