Mechanical Properties Metric English Comments
Tensile Strength 40.0 - 65.0 MPa
5800 - 9430 psi
Compression; ISO 527
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..