Mechanical Properties Metric English Comments
Tensile Strength >= 931 MPa

@Treatment Temp. 621 °C,
Time 14400 sec
>= 135000 psi

@Treatment Temp. 1150 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..