Mechanical Properties Metric English Comments
Tensile Strength 63.7 MPa
9250 psi
50 mm/min; ISO 527
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 63.7 MPa
9250 psi
Taiwan Sheen Soon Sheenthane® A9313H Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 63.7 MPa
9250 psi
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 63.7 MPa
9250 psi
ASTM D638
Samyang Trimma® FT6125 I[R] PMMA, Transparent
High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang.
Tensile Strength 63.7 MPa
9250 psi
ASTM D638
Samyang Trirex® 3017PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang.
Tensile Strength 63.7 MPa
9250 psi
ASTM D638
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and..
Tensile Strength 63.7 MPa
9250 psi
ASTM D638
Samyang Triloy® 450N Polymer Alloy, Blow Molding
Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang.