Polymer Property : Tensile Strength = 9020 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 55.3 - 62.2 MPa
8020 - 9020 psi
ASTM D882
OCTAL DPET™ PET Sheet
Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechan..