Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.846 MPa | 1428 psi | Silicone Property; ASTM D412 |
Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Desi.. |