Polymer Property : Tensile Strength = 9.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 9.30 MPa
1350 psi
Momentive Performance Materials TUFELâ„¢ II 94305 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 9.30 MPa
1350 psi
Momentive Performance Materials TUFELâ„¢ II 94306 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 9.30 MPa
1350 psi
Momentive Performance Materials FSE7570-D1 Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 9.30 MPa
1350 psi
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer
KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..