Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.615 MPa | 89.2 psi | ISO 7214 1998 |
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Tensile Strength | 0.615 MPa | 89.2 psi | ISO 7214 1998 |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |