Polymer Property : Tensile Strength = 870 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 870 MPa
126000 psi
H.C. Starck HPM 1760 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
Tensile Strength 870 MPa
126000 psi
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet
Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo..