Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 586 MPa @Temperature 22.8 °C |
85000 psi @Temperature 73.0 °F |
ASTM D3039 |
Quadrant EPP Ketron® LSG CC PEEK Ketron PEEK with 57% Woven Carbon Fiber |
|||
Tensile Strength | 586 - 689 MPa @Thickness >=25.4 mm |
85000 - 100000 psi @Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength | 586 - 689 MPa @Thickness >=25.4 mm |
85000 - 100000 psi @Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |