Polymer Property : Tensile Strength = 8.129 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.129 MPa
1179 psi
ASTM D412
Arlon T2020-R004 0.020" (0.508 mm) Cured Self-Fusing Silicone Rubber
Description: 1 inch wide x 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyethylene Product: Cured Self-Fusing Silicone RubberCross-Secti..