Mechanical Properties Metric English Comments
Tensile Strength 54.936 MPa
7967.8 psi
ASTM D638
E-Polymers TEKASTER® F101F Fast cycle time PBT
Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good..