Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 79.0 MPa | 11500 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Tensile Strength | 79.0 MPa @Temperature 23.0 °C |
11500 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |