Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 53.955 MPa | 7825.5 psi | ASTM D638 |
E-Polymers TEKASTER® F100 low-mid viscosity PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |