Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 53.5 MPa | 7760 psi | ISO 527 |
IPB Veralite® 100 Transparent APET Sheet Used in display applications such as kiosks, POP displays, signage; industrial applications such as guards, dispensers, and windows, and architecture. It posses these attributes:excellent impact re.. |
|||
Tensile Strength | 53.5 MPa | 7760 psi | ISO 527 |
IPB Veralite® 100AR Antireflective Transparent APET Sheet Antireflective has one matte surface and improved scratch resistance over Veralite®100. Used in display applications such as kiosks, POP displays, signage. It posses these attributes:excellent .. |