Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 0.517 MPa | >= 75.0 psi | ASTM D3574-75 Test E |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Tensile Strength | >= 0.517 MPa | >= 75.0 psi | ASTM D3573 Test E |
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Tensile Strength | >= 0.517 MPa | >= 75.0 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |