Polymer Property : Tensile Strength = 7400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 36.0 - 51.0 MPa
5220 - 7400 psi
ASTM D638
Huntsman RenShape® SL 7820 Stereolithography Plastic
RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear..