Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 710 MPa
103000 psi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..