Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 7.832 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.832 MPa
1136 psi
Silicone Property; Arlon SQA-TMS-009
Arlon 920-05B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular 0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Sel..
Tensile Strength 7.832 MPa
1136 psi
Silicone Property; Arlon SQA-TMS-009
Arlon 920-10B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..
Copyright © lookpolymers.com All Rights Reserved