Polymer Property : Tensile Strength = 7.557 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.557 MPa
1096 psi
Tape Property; ASTM D412
Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner
Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product..