Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.081 MPa | 1027 psi | Silicone Property; ASTM D412 |
Arlon LW3015B##-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.5 inch wide, 30 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll leng.. |