Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.067 MPa | 1025 psi | Silicone Property; ASTM D412 |
Arlon LW401R##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Tensile Strength | 7.067 MPa | 1025 psi | Silicone Property; ASTM D412 |
Arlon LW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Tensile Strength | 7.067 MPa | 1025 psi | Silicone Property; ASTM D412 |
Arlon LW401R##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |