Tensile Strength 696 MPa
101000 psi
Heat Treated
Weartech International WT-21 Cobalt Hardfacing & Wear Resistant Alloy
Applications: hot trimming & forging dies, high pressure high temperature valves, hot shears, valve seats, pump impellers, ringsInformation provided by Weartech International