Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.60 MPa | 667 psi | ISO 37 |
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound |
|||
Tensile Strength | 4.60 MPa | 667 psi | ISO 37 |
AlphaGary Evoprene™ GC 5656 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Tensile Strength | 4.60 MPa | 667 psi | ISO 37 |
AlphaGary Evoprene™ GC 5688 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |