Polymer Property : Tensile Strength = 6260 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 43.1 MPa
6260 psi
ASTM D412
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Tensile Strength 43.1 MPa
6260 psi
ASTM D638
GRECO ISOPAK 547HF ABS Resin
High Flow GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.