Polymer Property : Tensile Strength = 62.49 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 62.49 MPa
9063 psi
ASTM D638
E-Polymers TEKANATE® G7020 General Purpose Easy Molding Polycarbonate
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows ..