Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 38.06 MPa | 5520 psi | ASTM D-412 |
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati.. |