Polymer Property : Tensile Strength = 55000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 241 - 379 MPa
35000 - 55000 psi
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00)
C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated..
Tensile Strength 241 - 379 MPa
35000 - 55000 psi
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper A(TB00)
C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated..