Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 36.5 MPa | 5290 psi | ASTM D412 |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |