Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.65 MPa @Strain 100 % |
529 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B70CA Polyvinyl Chloride, Flexible (PVC, Flexible) Improved adhesion.Information provided by PolyOne |
|||
Tensile Strength | 3.65 MPa @Strain 100 % |
529 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B70CB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |