Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.6297 MPa | 526.44 psi | ASTM D412 |
E-Polymers EFLEX® V1040 EPDM/TPV V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq.. |