Mechanical Properties Metric English Comments
Tensile Strength 0.353 MPa
51.2 psi
ISO 7214 1998
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..